In plastic injection molding, the ability of a product to "smoothly demold" determines its yield and appearance. A draft angle that is too small can easily leave scratches, whitening, or ejector pin marks on the surface, and may also cause jamming due to insufficient ejection force. The main factors affecting demolding include the draft angle, the bonding pressure caused by material shrinkage, surface roughness, and the vacuum effect during demolding. This article breaks down the calculations and settings into actionable steps from an engineering perspective: first, it uses a simple method to roughly determine the required demolding force; second, it selects the draft angle based on the surface and material; third, it uses quantifiable contact pressure limits to configure the ejection area and the number of ejector pins; and finally, it provides methods to avoid scratches.
How to choose the draft angle
The principle is simple: the stickier the material, the rougher the surface, and the deeper the structure, the larger the draft angle should be. The table below provides suggestions for "angles on each side," which are easy to remember and implement.
Commonly Used Materials × Basic Angles of Surface Treatment
| Materials/Surfaces | Mirror polishing | Fine polishing | Shallow etching/sandblasting | Medium to deep etch marks |
|---|---|---|---|---|
| PP, PE | 0.5–1.0° | 1.0–1.5° | 1.5–2.0° | 2.5–4.0° |
| ABS, HIPS | 0.5–1.0° | 1.0–1.5° | 1.5–2.5° | 3.0–5.0° |
| PC, PMMA | 0.25–0.5° | 0.5–1.0° | 1.5–2.5° | 3.0–5.0° |
| POM | 0.5–1.0° | 1.0–1.5° | 1.5–2.0° | 2.5–4.0° |
| PA6/66 | 0.5–1.0° | 1.0–1.5° | 1.5–2.5° | 3.0–4.0° |
- Draft angle adjustment: For every 10 mm increase in draft depth, add an additional 0.3–0.5°. For depths > 25 mm, add an additional 0.5–1.0°.
- Texture cornering: For every 10 μm of texture depth, an additional 0.5° can be added; for deep textures ≥60 μm, an overall angle of 3–5° is recommended.
- Conservative approach to appearance: It is better to add corners during the design phase and then confirm the visual appearance with mold flow and prototypes; adding corners later is usually more costly.
How to make structural design user-friendly?
The draft angle isn't a one-size-fits-all issue; different structures require different strategies. Let's explain the common features in detail below:
- Rib: 0.5–1.0° on each side, rib thickness ≤ nominal wall thickness 0.5–0.6; add R0.3–0.5 at the rib root to reduce strain. Deep ribs (>20 mm) add another 0.5°.
- Boss: 1–2° on the outer side, 0.5–1° on the inner side. For deep holes or screw studs, use sleeve ejection or stripper plate instead of small ejector pins to force the screw out.
- Buckles/Barbs: The bevel of the buckle should be 1–2° and rounded; use a slider or angled top if possible, rather than forcibly pulling it out.
- Opening/window: 0.5–1° on each side of the hole wall; hole corner guide R0.3–0.8, the ejection mark will be fainter.
- Large flat surfaces: Do not rely solely on point-like ejector pins; instead, use stripping plates or large-area push plates to distribute force and significantly reduce whitening.
How to match the top exhaust with the exhaust?
Step 1: First select the correct ejection method
- Thin-shell and large-surface → Stripping plate/push plate preferred.
- For cylindrical bosses and deep holes, sleeve ejection is safer than small ejector pins.
- For buckles and partial undercuts, use the angled top/slider to detach them; do not use a pin to pull them apart forcefully.
Step 2: Number and position of the top points
First check the dimensions, then decide on the number of points:
- For small items ≤ 50 mm: place them at 3 points, and try to avoid the front appearance area.
- 50–100 mm: Place 5 points (1 at each of the four corners + 1 at the center or where the ribs intersect).
- 100–200 mm: at least 8 points; for large flat plates/thin shells, adding a small push plate or using a stripper plate directly will make it more stable.
Where should I put the dot?
- Prioritize placing it near "where the fibers meet, where the material is thick, and near the rounded corners" (these areas can hold their shape and are less prone to whitening).
- Avoid using glossy surfaces if possible; if you really can't avoid them, place them on the inside or in an inconspicuous place.
Spacing and distance from the edge (safe distance to avoid localized whitening):
- ≥ 6–10 mm from the outer edge (too close to the edge can easily cause edge chipping/whitening).
- The spacing between them should be 20–40 mm (the thinner the material, the denser it should be; the thicker the material, the sparser it can be).
What to do if you have to place it on a smooth surface:
- Use a flat-headed, large-diameter thimble (to distribute the force).
- Make fine oil grooves/shallow textures on the mold surface to reduce adhesion.
- It would be even better if the push plate/stripping plate could be modified.
Step 3: Eliminate the vacuum effect in advance
- Adding micro-venting grooves (0.01–0.02 mm deep, 1–3 mm wide) or creating vacuum-breaking points (very shallow grooves/small notches) on the end face will prevent it from sticking.
- Venting paths must be provided at the end of the gate, the thick protrusion, and the top of the gate; the venting is only effective if it can be opened to the atmosphere.
Timing and speed of ejection
- Wait until the gate is sealed and the surface is firm before ejecting; ejecting too early is most likely to cause whitening.
- Start slowly and then accelerate: "loosen" the contact surface before accelerating; eject in stages if necessary.
| Phenomenon | Common causes | Immediate countermeasures |
|---|---|---|
| Whitening around the thimble | Ejector pin too small/too sharp, misposition, ejection too early, low mold temperature | Replace with a flat-headed large ejector pin or add a push plate; delay ejection and increase mold temperature by 5–10°C; move the ejector pin to the rib intersection or thick area. |
| Strain along the draft direction | Insufficient release angle, deep etching, undercuts or scale buildup on the surface | Add 0.5–1° to each side; modify the texture or polish; clean the mold and add radius; replace hard pull with sliders/angled ejectors. |
| The mold in the local area cannot be pushed up. | Vacuum adsorption, poor exhaust, uneven wall thickness, shrinkage and jamming | Micro-venting grooves are opened on the end face; venting is opened at the air trapping point; cooling is added to the thick area/the wall thickness is changed. |
| The thimble mark is visible. | Concentrated stress, insufficient area, and hard top surface | Increase the number of ejector pins or modify the ejector plate; move the ejector pins to a non-visual surface; use a stripper plate on the outer surface. |
| Multiple white powdery marks | Ejection too fast/too early, mold temperature too low | Reduce initial velocity and eject in stages; increase mold temperature; ensure gate sealing before ejecting. |
Tips for machining and surface treatment
- The polishing direction should be consistent with the draft direction. It is easiest to scratch white marks when burrs or brush marks are in the opposite direction.
- Surface coatings (nitriding, DLC) can reduce adhesion, which is very beneficial for long-cycle mass production.
- Release agents should only be used as a verification tool and should not be relied upon; a more ideal approach is to add angles, modify ejection mechanisms, and add venting.
- R-angle reduction: sharp corners are reduced to R0.3–0.8, resulting in smoother demolding and less visible marks.
- Maintenance: Regularly clean the etched pores and venting grooves to remove accumulated dirt; old grease is like an "invisible barb".
Material and surface dimensions: Refer to a table to determine the basic angle → Add angles based on depth and texture → Select the correct ejection method and venting → Control ejection timing and speed. Standardize this process into a checklist, and combine it with your company's existing materials and mold temperature conditions. Over the long term, this will not only reduce whitening and tearing, but also minimize the number of trial moldings and improvement time. In short, designing a "good demolding" structure first, and then fine-tuning the molding parameters, will result in much more stable production.